Items where Research Institute, Centre or Group is "Centre for Corrosion Technology"

[Atom feed] Atom [RSS2 feed] RSS
Group by: Creators | Year | Item Type | Full Text | No Grouping
Jump to: 2018 | 2017 | 2016 | 2015 | 2014 | 2013 | 2012 | 2011 | 2010 | 2009 | 2008 | 2007 | 2006 | 2005 | 2004 | 2003 | 2002 | 2001 | 2000 | 1999 | 1998 | 1997 | 1996 | 1994 | 1991 | 1990
Number of items at this level: 253.

2018

file
AL-MOUSSAWI, M and SMITH, Alan (2018). Defects in Friction Stir Welding of Steel. Metallography, Microstructure, and Analysis, 7, 194-202. [Article]

file
AL-MOUSSAWI, M. and SMITH, Alan (2018). Thermo-Mechanical Effect on Poly Crystalline Boron Nitride Tool Life During Friction Stir Welding (Dwell Period). Metals and Materials International, 24 (3), 560-575. [Article]

file
AL-MOUSSAWI, M. A. M. (2018). A study on the failure of steel chains in rotary cement kilns. Metallography, Microstructure, and Analysis, 7 (2), 153-167. [Article]

ALEXOPOULOS, Nikolaos D, MIGKLIS, Evangelos and MYRIOUNIS, Dimitrios (2018). Experimental analysis of constant-amplitude fatigue properties in 6156 (Al-Mg-Si) sheet aluminum alloy. The Journal of Strain Analysis for Engineering Design, 53 (8), 676-686. [Article]

2017

file
AL-MOUSSAWI, M., SMITH, Alan and FARAJI, M. (2017). Friction stir welding of EH46 steel grade at dwell stage: Microstructure evolution. Metallography, Microstructure, and Analysis, 6 (6), 489-501. [Article]

file
AL-MOUSSAWI, M., SMITH, Alan, YOUNG, Andrew E, CATER, S. and FARAJI, M. (2017). Modelling of friction stir welding of DH36 steel. The International Journal of Advanced Manufacturing Technology, 92 (1-4), 341-360. [Article]

file
AMJAD, Khurram, ASQUITH, David, EANN, Patterson, SEBASTIAN, Chris and WANG, Wei-Chun (2017). The interaction of fatigue cracks with a residual stress field using thermoelastic stress analysis and synchrotron X-ray diffraction experiments. Royal Society Open Science, 4 (171100). [Article]

file
JAMES, Malcolm Neil, HATTINGH, Danie, ASQUITH, David, NEWBY, Mark and DOUBELL, Phillip (2017). Residual stresses in condition monitoring and repair of thermal power generation components. Theoretical and Applied Fracture Mechanics, 92, 289-297. [Article]

NGO, Son, LOWE, Chris, LEWIS, Oliver and GREENFIELD, David (2017). Development and optimisation of focused ion beam/scanning electron microscopy as a technique to investigate cross sections of organics coatings. Progress in Organic Coatings, 106, 33-40. [Article]

filefile
PASCUAL-GONZALEZ, Cristina, SCHILEO, Giorgio, KHESRO, Amir, STERIANOU, Iasmi, WANG, Dawei, REANEY, Ian and FETEIRA, Antonio (2017). Band gap evolution and piezoelectric-to-electrostrictive crossover in (1-x)KNbO3-x(Ba0.5Bi0.5)(Nb0.5Zn0.5)O3 ceramics. Journal of Materials Chemistry C, 5 (8), 1990-1996. [Article]

PASCUAL-GONZALEZ, Cristina, STERIANOU, Iasmi and FETEIRA, Antonio (2017). Evolution of piezoelectric response in (1-x)KNbO3-x(Ba0.5Bi0.5)(Nb0.5Zn0.5)O3 ceramics. In: GEORGE, Thomas, DUTTA, Achyut K. and ISLAM, M. Saif, (eds.) Micro- and Nanotechnology Sensors, Systems, and Applications IX. SPIE Proceedings (10194). SPIE Publications, p. 1019430. [Book Section]

file
WANG, Dawei, HUSSAIN, Fayaz, KHESRO, Amir, FETEIRA, Antonio, TIAN, Ye, ZHAO, Quanliang, REANEY, Ian M. and ZHANG, S. (2017). Composition and Temperature Dependence of Structure and Piezoelectricity in (1−x)(K1−yNay)NbO3-x(Bi1/2Na1/2)ZrO3Lead-Free Ceramics. Journal of the American Ceramic Society, 100 (2), 627-637. (In Press) [Article]

2016

file
AL-MOUSSAWI, M., SMITH, Alan, YOUNG, Andrew E, FARAJI, M. and CATER, S. (2016). An advanced numerical model of friction stir welding of DH36 steel. In: 11th International Symposium on Friction Stir Welding, TWI, Cambridge, 17-19 May 2016. (In Press) [Conference or Workshop Item]

filefile
KHESRO, Amir, WANG, Dawei, HUSSAIN, Fayaz, SINCLAIR, Derek, FETEIRA, Antonio and REANEY, Ian (2016). Temperature Stable and Fatigue Resistant lead-free ceramics for actuators. Applied Physics Letters, 109 (14), p. 142907. [Article]

filefile
MAY, M, WANG, Heming and AKID, Robert (2016). Influence of adding multiwalled carbon nanotubes on the adhesive strength of composite epoxy/sol–gel materials. Journal of Coatings Technology and Research, 13 (2), 325-332. [Article]

filefile
PASCUAL-GONZALEZ, Cristina, SCHILEO, Giorgio and FETEIRA, Antonio (2016). Band gap narrowing in ferroelectric KNbO3-Bi(Yb,Me)O3 (Me=Fe or Mn) ceramics. Applied Physics Letters, 109 (13). [Article]

file
WANG, Dawei, HUSSAIN, Fayaz, KHESRO, Amir, FETEIRA, Antonio, TIAN, Ye, ZHAO, Quanliang and REANEY, Ian (2016). Composition and temperature dependence of structure and piezoelectricity in (1−x)(K1−yNay)NbO3-x(Bi1/2Na1/2)ZrO3 lead-free ceramics. Journal of the American Ceramic Society, 100 (2), 627-637. [Article]

file
WANG, Dawei, KHESRO, Amir, MURAKAMI, S, FETEIRA, Antonio, ZHAO, Quanliang and REANEY, Ian M. (2016). Temperature dependent, large electromechanical strain in Nd-doped BiFeO3-BaTiO3 lead-free ceramics. Journal of the European Ceramic Society. [Article]

filefile
WANG, Heming, RAHAQ, Yaqub and KUMAR, Vikas (2016). A composite light-harvesting layer from photoactive polymer and halide perovskite for planar heterojunction solar cells. Scientific Reports, 6 (29567), 1-9. [Article]

2015

file
GALEHDARI, S.A., KADKHODAYAN, M. and HADIDI-MOUD, Saeid (2015). Analytical, experimental and numerical study of a graded honeycomb structure under in-plane impact load with low velocity. International Journal of Crashworthiness, 20 (4), 387-400. [Article]

file
LEWIS, Oliver, RADLEY, Keith, BRAMHALL, Mike and METCALF, John (2015). Student produced media and the use of web based sites for the assessment of technical and communication skills in engineering students. In: 9th International Conference on New Horizons in Industry, Business and Education, Skiathos Palace Hotel, Skiathos, Greece, 27-28 August 2015. [Conference or Workshop Item]

file
MAGOWAN, Stephen, BRAMHALL, Mike and LEWIS, Oliver (2015). Portfolio assessment of laboratory practicals integrating learning across modules. In: 9th International Conference on New Horizons in Industry, Business and Education, Skiathos Palace Hotel, Skiathos, Greece, 27-28 August 2015. [Conference or Workshop Item]

file
OLUSOLA, O.I., MADUGU, M.L., ABDUL-MANAF, N.A. and DHARMADASA, I (2015). Growth and characterisation of n- and p-type ZnTe thin films for applications in electronic devices. Current Applied Physics, 16 (2), 120-130. [Article]

file
SCHILEO, Giorgio, FETEIRA, Antonio, REICHMANN, Klaus, LI, Ming and SINCLAIR, Derek (2015). Structure–property relationships in (1 − x)BaTiO3–xBiGdO3 ceramics. Journal of the European Ceramic Society, 35 (9), 2479-2488. [Article]

file
WANG, Heming and KUMAR, Vikas (2015). Transparent and conductive polysiloxanes/ PEDOT:PSS nanocomposite thin films with a “water-impermeable” property to significantly enhance stability of organic–inorganic hybrid solar cells. RSC Advances, 5 (13), 9650-9657. [Article]

2014

BINGHAM, Paul, HANNANT, O.M., REEVES-MCLAREN, N., STENNETT, M.C. and HAND, R.J. (2014). Selective behaviour of dilute Fe3+ ions in silicate glasses: an Fe K-edge EXAFS and XANES study. Journal of Non-Crystalline Solids, 387, 47-56. [Article]

DHARMADASA, I, BINGHAM, Paul, ECHENDU, O., SALIM, H., DRUFFEL, T., DHARMADASA, R., SUMANASEKERA, G., DHARMASENA, R., DERGACHEVA, M., MIT, K., URAZOV, K., BOWEN, L., WALLS, M. and ABBAS, A. (2014). Fabrication of CdS/CdTe-Based thin film solar cells using an electrochemical technique. Coatings, 4 (3), 380-415. [Article]

ECHENDU, O.K., FAUZI, F., WEERASINGHE, A.R. and DHARMADASA, I. (2014). High short-circuit current density CdTe solar cells using all-electrodeposited semiconductors. Thin Solid Films, 556, 529-534. [Article]

ECHENDU, O.K., FAUZI, F., WEERASINGHE, A.R. and DHARMADASA, I. (2014). High short-circuit current density CdTe solar cells using all-electrodeposited semiconductors. Thin Solid Films, 556, 529-534. [Article]

FLETCHER-WOOD, R.L., GORIN, Colin, FORDER, Sue, BINGHAM, Paul and HRILJAC, J.A. (2014). Mössbauer spectroscopy for optimising systems for environmental remediation. Hyperfine Interactions, 226 (1-3), 499-508. [Article]

HYATT, N.C., SCHWARZ, R.R., BINGHAM, Paul, STENNETT, M.C., CORKHILL, C.L., HEATH, P.G., HAND, R.J., JAMES, M., PEARSON, A. and MORGAN, S. (2014). Thermal treatment of simulant plutonium contaminated materials from the Sellafield site by vitrification in a blast-furnace slag. Journal of Nuclear Materials, 444 (1-3), 186-199. [Article]

KUMAR, Vikas, WANG, Heming and RODENBURG, Cornelia (2014). High-efficiency inverted polymer solar cells via dual effects of introducing the high boiling point solvent and the high conductive PEDOT:PSS layer. Organic Electronics, 15 (9), 2059-2067. [Article]

MADUGU, M. L., BOWEN, L., ECHENDU, O. K. and DHARMADASA, I (2014). Preparation of indium selenide thin film by electrochemical technique. Journal of Materials Science: Materials in Electronics, 25 (9), 3977-3983. [Article]

RODELLA, N., BOSIO, A., ZACCO, A., BORGESE, L., PASQUALI, M., DALIPI, R., DEPERO, L.E., PATEL, V., BINGHAM, Paul and BONTEMPI, E. (2014). Arsenic stabilization in coal fly ash through the employment of waste materials. Journal of Environmental Chemical Engineering, 2 (3), 1352-1357. [Article]

SCHILEO, Giorgio, FETEIRA, Antonio, REANEY, Ian M., POSTOLACHE, Petronel, MITOSERIU, Liliana and REICHMANN, Klaus (2014). Characterization of Yttrium Iron Garnet/Barium Titanate Multiferroic Composites Prepared by Sol-Gel and Coprecipitation Methods. International Journal of Applied Ceramic Technology, 11 (3), 457-467. [Article]

SULEIMAN, R, KHALED, M, WANG, H., SMITH, T. J., GITTENS, J, AKID, R., MOHAMED EL ALI, B and KHALIL, A (2014). Comparison of selected inhibitor doped sol–gel coating systems for protection of mild steel. Corrosion engineering science and technology, 49 (3), 189-196. [Article]

WONG, Kevin, FOX, Chris and ALBERTSON, Kevin (2014). Justice reinvestment in an "Age of Austerity" : developments in the United Kingdom. Victims & Offenders, 9 (1), 76-99. [Article]

WRIGHT, Adrian C, CLARKE, Stuart J, HOWARD, Christopher K, BINGHAM, Paul, FORDER, Sue, HOLLAND, Diane, MARTLEW, David and FISCHER, Henry E (2014). The environment of Fe2+/Fe3+ cations in a soda–lime–silica glass. Physics and Chemistry of Glasses : European Journal of Glass Science and Technology Part B, 55 (6), 243-252. [Article]

2013

BRYANT, David E., GREENFIELD, David, WALSHAW, Richard D., JOHNSON, Benjamin R.G., HERSCHY, Barry, SMITH, Caroline, PASEK, Matthew A., TELFORD, Richard, SCOWEN, Ian, MUNSHI, Tasnim, EDWARDS, Howell G.M., COUSINS, Claire R., CRAWFORD, Ian A. and KEE, Terence P. (2013). Hydrothermal modification of the Sikhote-Alin iron meteorite under low pH geothermal environments. A plausibly prebiotic route to activated phosphorus on the early Earth. Geochimica et Cosmochimica Acta, 109, 90-112. [Article]

DELUCA, Marco, SCHUETZ, Denis, AKSEL, Elena, PICHT, G, FORONDA, H, FETEIRA, Antonio, REICHMANN, Klaus, WEBBER, K and JONES, Jacob (2013). Raman spectroscopy of Sodium Bismuth Titanate ceramics. In: International Ultrasonics Symposium International Symposium on the Applications of Ferroelectrics Joint International Frequency Control Symposium European Frequency and Time Forum, Prague, Czech Republic, 21-25th July 2013. (Unpublished) [Conference or Workshop Item]

DENIS ROMERO, Fabio, GIANOLIO, Diego, CIBIN, Giannantonio, BINGHAM, Paul, D’HOLLANDER, Jeanne-Clotilde, FORDER, Sue and HAYWARD, Michael A. (2013). Topochemical reduction of the Ruddlesden–Popper Phases Sr2Fe0.5Ru0.5O4and Sr3(Fe0.5Ru0.5)2O7. Inorganic Chemistry, 52 (19), 10920-10928. [Article]

FETEIRA, Antonio, LUISMAN, Luke, SCHILEO, Giorgio, DELUCA, Marco and REICHMANN, Kaus (2013). Structure-property relationships in BaTiO3-BiFeO3-BiYbO3 Ceramics. In: Ceramic Interconnect and Ceramic Microsystems Technologies (CICMT 2013)., Orlando, USA, 23-26th April 2013. (Unpublished) [Conference or Workshop Item]

JABBAL, M., LIDDLE, S., POTTS, Jonathan and CROWTHER, W. (2013). Development of design methodology for a synthetic jet actuator array for flow separation control applications. Proceedings of the Institution of Mechanical Engineers, Part G: Journal of Aerospace Engineering, 227 (1), 110-124. [Article]

KUMAR, Vikas and WANG, Heming (2013). Plasmonic Au nanoparticles for enhanced broadband light absorption in inverted organic photovoltaic devices by plasma assisted physical vapour deposition. Organic Electronics, 14 (2), 560-568. [Article]

MAY, Mousa, WANG, Heming and AKID, Robert (2013). Bond strength of hybrid sol–gel coatings with different additives. Journal of Coatings Technology and Research, 10 (3), 407-413. [Article]

MYRIOUNIS, Dimitrios (2013). Microdeformation Behaviour of Al/SiCp Composites. LAP LAMBERT Academic Publishing. [Authored Book]

REICHMANN, Klaus, KRAUSS, Werner, SCHUETZ, Denis, NADERER, Michael, DELUCA, Marco, SUPANCIC, P, FETEIRA, Antonio and KAINZ, Theresa (2013). Bismuth-Alkali-Titanate based ceramics for piezoelectric actuator applications. In: Ceramic Interconnect and Ceramic Microsystems Technologies (CICMT 2013, Orlando, USA, 23-26th April 2013. (Unpublished) [Conference or Workshop Item]

file
SCHILEO, Giorgio, DIAS, Aanderson, MOREIRA, Roberto L., JACKSON, Tim J., SMITH, Paul A., CHUNG, Kelvin T.S. and FETEIRA, Antonio (2013). Structure and microwave dielectric properties of low firing Bi2Te2W3O16 ceramics. Journal of the American Ceramic Society, 97 (4), 1096-1102. [Article]

SCHILEO, Giorgio, FETEIRA, Antonio, POSTOLACHE, Petronel, LILIANA, Mitoseriu and REICHMANN, Klaus (2013). Synthesis and characterization of novel multiferroic composites based on Y3Fe5O12@BaTiO3 and Y3Fe5O12@Pb(Zr,Ti)O3. In: Ceramic Interconnect and Ceramic Microsystems Technologies (CICMT 2013), Orlando, USA, 23-26th April 2013. (Unpublished) [Conference or Workshop Item]

SCHILEO, Giorgio, FETEIRA, Antonio and REICHMANN, Klaus (2013). Synthesis and Characterization of Core-Shell Multiferroic Nanocomposites Based on Y3Fe5O12 and BaTiO3/Pb(Zr,Ti)O3. In: Ferroelectrics UK 2013, Sheffield, 17-18th January 2013. (Unpublished) [Conference or Workshop Item]

SCHILEO, Giorgio, FETEIRA, Antonio, SHIMIZU, T and REICHMANN, Klaus (2013). Synthesis and characterization of multiferroic ceramic composites based on Y3Fe5O12/BaTiO3 and Y3Fe5O12/Pb(Zr,Ti)O3. In: Materials Science and Technology 2013, Montreal, Canada, 27-31 October 2013. (Unpublished) [Conference or Workshop Item]

SCHILEO, Giorgio, LUISMAN, Luke, FETEIRA, Antonio, DELUCA, Marco and REICHMANN, Klaus (2013). Structure-property relationships in BaTiO3-BiFeO3-BiYbO3 ceramics. Journal of the European Ceramic Society, 33 (8), 1457-1468. [Article]

SETH, Sampan, JONES, Hywel and LEWIS, Oliver (2013). Wear resistance performance of thermally sprayed Al-Ti alloy measured by three body micro-scale abrasive wear test. Wear, 302 (1-2), 972-980. [Article]

VIKAS, Kumar and WANG, Heming (2013). Selection of metal substrates for completely solution-processed inverted organic photovoltaic devices. Solar Energy Materials and Solar Cells, 113, 179-185. [Article]

2012

ALI, M.A., HASAN, Syed and MYRIOUNIS, Dimitrios (2012). A method of analysis to estimate thermal down-shock stress profiles in hollow cylinders when subjected to transient heat/cooling cycle. In: YIGIT, Faruk and HASHMI, Mohammed S.J., (eds.) Materials and Manufacturing Technologies. Advanced Materials Research, XIV (445). Switzerland, Trans Tech Publications Ltd., 893-898. [Book Section]

BINGHAM, Paul and BARNEY, E R (2012). Structure of iron phosphate glasses modified by alkali and alkaline earth additions: neutron and x-ray diffraction studies. Journal of Physics: Condensed Matter, 24 (17), p. 175403. [Article]

BINGHAM, Paul, HYATT, N. C. and HAND, R. J. (2012). Vitrification of UK intermediate level radioactive wastes arising from site decommissioning : property modelling and selection of candidate host glass compositions. Glass technology, 53 (3), 83-100. [Article]

CHEN, Yao-Chang, REEVES-MCLAREN, Nik, BINGHAM, Paul, FORDER, Sue and WEST, Anthony R. (2012). Synthesis and characterization of Li11Nd18Fe4O39−δ. Inorganic Chemistry, 51 (15), 8073-8082. [Article]

CICEK, B., ESPOSITO, L., TUCCI, A., BERNARDO, E., BOCCACCINI, A.R. and BINGHAM, Paul (2012). Microporous glass ceramics from combination of silicate, borate and phosphate wastes. Advances in Applied Ceramics, 111 (7), 415-421. [Article]

FATOBA, Olusegun, AKID, R, MYRIOUNIS, Dimitrios and CURIEL-SOSA, Jose Luis (2012). Lifetime modelling for corrosion fatigue. In: National Student Conference in Metallic Materials 2012, Manchester Conference Centre and Hotel, Manchester, 25-26 June 2012. (Unpublished) [Conference or Workshop Item]

HASAN, Syed (2012). Biaxial themal down shock analysis of a thin 316 stainless steel plate. In: NuMat 2012 : the Nuclear Materials Conference, Osaka, Japan, 22-25 October 2012. (Submitted) [Conference or Workshop Item]

HASAN, Syed (2012). Fatigue behaviour of robbed steel structures. In: 15th International Conference on Advances in Materials and Processing Technologies (AMPT 2012), Wollongong, Australia, 23-26 September 2012. (Unpublished) [Conference or Workshop Item]

HASAN, Syed and NASSER, M.A. (2012). Elastic-Plastic thermal shock analysis. In: NuMat 2012 : the Nuclear Materials Conference, Osaka, Japan, 22-25 October 2012. (Submitted) [Conference or Workshop Item]

KALANTARI, Kambiz, STERIANOU, Iasmi, SINCLAIR, Derek C., BINGHAM, Paul, POKORNÝ, Jan and REANEY, Ian M. (2012). Structural phase transitions in Ti-doped Bi1-xNdxFeO3 ceramics. Journal of Applied Physics, 111 (6), 064107. [Article]

LEWIS, Oliver, CRITCHLOW, Gary, WILCOX, Geoffrey, DEZEEUW, Ard and SANDER, Joerg (2012). A study of the corrosion resistance of a waterborne acrylic coating modified with nano-sized Titanium Dioxide. Progress in Organic Coatings, 73 (1), 88-94. [Article]

MCGANN, O.J., BINGHAM, Paul, HAND, R.J., GANDY, A.S., KAVČIČ, M., ŽITNIK, M., BUČAR, K., EDGE, R. and HYATT, N.C. (2012). The effects of γ-radiation on model vitreous wasteforms intended for the disposal of intermediate and high level radioactive wastes in the United Kingdom. Journal of Nuclear Materials, 429 (1-3), 353-367. [Article]

MYRIOUNIS, Dimitrios and HASAN, Syed (2012). Fatigue behaviour of Al/Al203 metal matrix composites. In: ECF19 - 19th European Conference on Fracture, Kazan Scientific Centre of the Russian Academy of Sciences, Kazan, Russia, 26-31 August 2012. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios, MATIKAS, T. E. and HASAN, Syed (2012). Fatigue behaviour of SiC particulate-reinforced A359 aluminium matrix composites. Strain, 48 (4), 333-341. [Article]

REICHMANN, Klaus, SCHUTZ, Denis, DELUCA, Marco and FETEIRA, Antonio (2012). Lone-pair effect in Bismuth Sodium Titanate based ceramics investigated by temperature dependent Raman spectrometry. In: International Workshop on Relaxor Ferroelectrics, Schloss Edesheim, Germany, 7-11th October 2012. (Unpublished) [Conference or Workshop Item]

SCHUTZ, Denis, DELUCA, Marco, KRAUSS, Werner, FETEIRA, Antonio and REICHMANN, Klaus (2012). Lone pair-induced covalency as the cause of temperature and field induced instabilities in Bismuth sodium titanate. In: Nature materials conference: Frontiers in Electronic materials: correlation effects and memristive phenomena, Aachen, 17-20 June 2012. (Unpublished) [Conference or Workshop Item]

SETH, Sampan, LEWIS, Oliver, JONES, Alan Hywel, STEPHENSON, Daniel, BODEN, Marcela and THISTLETHWAITE, Stuart (2012). A study of corrosion and wear resistance performance of thermally sprayed Al-Zn-In and Al-Ti alloy coatings. In: 53rd Corrosion Science Symposium, National Physical Laboratory, Teddington, UK, 6-7 September 2012. (Unpublished) [Conference or Workshop Item]

TAN, Chaou, FETEIRA, Antonio and SINCLAIR, Derek (2012). Ba2Bi1.4Nb0.6O6: a nonferroelectric, high permittivity oxide. Chemistry of Materials, 24 (12), 2247-2249. [Article]

WRIGHT, AdrianC., SINCLAIR, Roger N., SHAW, Joanna L., HAWORTH, Richard, MARASINGHE, G.Kanishka, DAY, Delbert E., BINGHAM, Paul, FORDER, Susan D., CUELLO, Gabriel J. and FISCHER, Henry J. (2012). The atomic and magnetic structure and dynamics of iron phosphate glasses. Physics and Chemistry of Glasses, 53 (6), 227-244. [Article]

ZHOU, Changrong, FETEIRA, Antonio, SHAN, Xu, YANG, Huabin, ZHOU, Qin, CHENG, Jun, LI, Weizhou and WANG, Hua (2012). Remarkably high-temperature stable piezoelectric properties of Bi(Mg0.5Ti0.5)O3 modified BiFeO3-BaTiO3 ceramics. Applied Physics Letters, 101 (3), 032901. [Article]

2011

AFELUMO, Adebola and HASAN, Syed (2011). Corrosion behaviour of closed cell metal foams in 3.5wt% NaCl at room temperature. In: National Student Conference in Metallic Materials 2011, Halifax Hall, The Endcliffe Village, Sheffield, 20 June 2011. (Unpublished) [Conference or Workshop Item]

AKID, R., GOBARA, M. and WANG, H. (2011). Corrosion protection performance of novel hybrid polyaniline/sol–gel coatings on an aluminium 2024 alloy in neutral, alkaline and acidic solutions. Electrochimica Acta, 56 (5), 2483-2492. [Article]

BERNARDO, E and BINGHAM, Paul (2011). Sintered silicophosphate glass ceramics from MBM ash and recycled soda-lime-silica glass. Advances in Applied Ceramics, 110 (1), 41-48. [Article]

BINGHAM, Paul, CONNELLY, A J, HYATT, N C and HAND, R J (2011). Corrosion of glass contact refractories for the vitrification of radioactive wastes: a review. International Materials Reviews, 56 (4), 226-242. [Article]

BINGHAM, Paul, CONNELLY, A.J., CASSINGHAM, N.J. and HYATT, N.C. (2011). Oxidation state and local environment of selenium in alkali borosilicate glasses for radioactive waste immobilisation. Journal of Non-Crystalline Solids, 357 (14), 2726-2734. [Article]

CASSINGHAM, Nathan J., STENNETT, Martin C., BINGHAM, Paul, HYATT, Neil C. and AQUILANTI, Giuliana (2011). The structural role of Zn in nuclear waste glasses. International Journal of Applied Glass Science, 2 (4), 343-353. [Article]

CONNELLY, A.J., HAND, R.J., BINGHAM, Paul and HYATT, N.C. (2011). Mechanical properties of nuclear waste glasses. Journal of Nuclear Materials, 408 (2), 188-193. [Article]

file
LEWIS, Oliver, O'FLAHERTY, Fin, LAMBERT, Paul, STEPHENSON, Dan, BODEN, M and THISTLETHWAITE, S (2011). A Study of Aluminium Zinc Indium Thermal Spray Coatings for the Protection of Steel Rebars in Reinforced Concrete. In: 5th RIPT (Les Recontres Internationales sur la Projection Themique), Limoges, France, 7-9 December 2011. [Conference or Workshop Item]

LEWIS, Oliver, SETH, Sampan, JONES, Alan Hywel, FARMILO, Nick, STEPHENSON, Daniel, BODEN, Marcela and THISTLETHWAITE, Stuart (2011). The development and optimization of aluminium alloys for thermal spray coating application to steel substrates. In: 5th RIPT (Les Recontres Internationales sur la Projection Themique), Limoges, France, 7-9 December 2011. (Unpublished) [Conference or Workshop Item]

LUISMAN, Luke, FETEIRA, Antonio and REICHMANN, Klaus (2011). Weak-relaxor behaviour in Bi/Yb-doped KNbO3 ceramics. Applied Physics Letters, 99 (19), p. 192901. [Article]

MATIKAS, T.E. and HASAN, Syed (2011). Deformation characteristics of aluminium composites for structural applications. In: AHMAD, Zaki, (ed.) Recent trends in processing and degradation of aluminium alloys. InTech, 347-370. [Book Section]

MYRIOUNIS, Dimitrios (2011). Fracture toughness of MMCs subjected to heat treatment - NDE. In: Second Greek=Ukranian Conference on Fracture Mechanics of Materials and Structures, Lviv, Ukraine, 3-7 October 2011. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios and HASAN, Syed (2011). Fatigue and fracture behaviour of Al-SiCp MMC NDE by IR detection. In: ICCM 18. the International Conference on Composite Materials, Jeju Island, Korea, 21-26 August 2011. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios and HASAN, Syed (2011). Fatigue crack growth behaviour of Al/SiC metal matrix composite. In: Deformation and Fracture of Composites (DFC-11) & Structural Integrity and Multi-scale Modelling (SI-5) : Celebrating 20 Years of DFC, A Joint Sheffield-Cambridge Conference, Queens' College Cambridge, 12-15 April 2011. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios and HASAN, Syed (2011). Fatigue life estimation of aluminium alloy reinforced with SiC particulates in annealed conditions. In: ICCM 18. the International Conference on Composite Materials, Jeju Island, Korea, 21-26 August 2011. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios, HASAN, Syed and BARE, T (2011). Fracture toughness behaviour of Aluminium 5xxx alloys - NDE by heatwave detection. In: 14th International Conference on Advances in Materials and Processing Technologies (AMPT 2011), Istanbul, Turkey, 13-16th July 2011. (Unpublished) [Conference or Workshop Item]

NASSER, M.A., HASAN, Syed and MYRIOUNIS, Dimitrios (2011). Numerical modelling analysis of isothermal fatigue. In: National Student Conference in Metallic Materials 2011, Halifax Hall, The Endcliffe Village, Sheffield, 20 June 2011. (Unpublished) [Conference or Workshop Item]

STRATHDEE, Tamsin, LUISMAN, Luke, FETEIRA, Antonio and REICHMANN, Klaus (2011). Ferroelectric-to-relaxor Crossover in (1-x) BaTiO3-xBiYbO3 (0≤ x≤ 0.08) ceramics. Journal of the American Ceramic Society, 94 (8), 2292-2295. [Article]

2010

BINGHAM, Paul, CONNELLY, A., HAND, R. and HYATT, N. (2010). Vitrification of legacy and intermediate level radioactive wastes : opportunities and challenges. Nuclear Future, 6 (6), 250-254. [Article]

BINGHAM, Paul, CONNELLY, A.J., HAND, R.J., HYATT, N.C., NORTHRUP, P.A., ALONSO MORI, R., GLATZEL, P., KAVCIC, M., ZITNIK, M., BUCAR, K. and EDGE, R. (2010). A multi-spectroscopic investigation of sulphur speciation in silicate glasses and slags. Glass technology, 51 (2), 63-80. [Article]

BRYANT, D. E., MARRIOTT, K. E. R., GREENFIELD, David, MACGREGOR, S. A., SMITH, C., PASEK, M. A. and KEE, T. (2010). The rise of chemical complexity from meteorite sources: Implications for origin-of-life studies. Origins of Life and Evolution of Biospheres, 40, p. 513. [Article]

BRYANT, D. E., MARRIOTT, K. E. R., GREENFIELD, David, MACGREGOR, S.A., SMITH, C., PASEK, M.A. and KEE, T. P. (2010). Special Issue: Abstracts from the 9th European Workshop on Astrobiology, Brussels, October 12–14, 2009. Origins of Life and Evolution of Biospheres, 40 (6), 499-607. [Article]

CASSINGHAM, N.J., STENNETT, M.C., BINGHAM, Paul, AQUILANTI, G. and HYATT, N.C. (2010). The role of Zn in model nuclear waste glasses studied by XAS. In: Diamond '10 Conference - Decommissioning, Immobilisation and Management of, Manchester, UK, 15-16 December 2010. [Conference or Workshop Item]

FETEIRA, Antonio, IDDLES, David, PRICE, Tim, MUIR, Duncan and REANEY, Ian M. (2010). High-permittivity and low-loss microwave dielectric ceramics based on (x)RE(Zn1/2Ti1/2)O3-(1−x)CaTiO3 (RE=La and Nd). Journal of the American Ceramics Society, 94 (3), 817-821. [Article]

FETEIRA, Antonio and REICHMANN, Klaus (2010). NTC Ceramics: Past, Present and Future. Advances in Science and Technology, 67, 124-133. [Article]

FETEIRA, Antonio, SINCLAIR, D. C. and LANAGAN, M. T. (2010). Effects of average and local structure on the dielectric behavior of (1−x)BaTiO[sub 3]–xLaYO[sub 3] (0≤x≤0.40) ceramics. Journal of Applied Physics, 108 (1), 014112. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C. and KREISEL, Jens (2010). Average and Local Structure of (1−x)BaTiO3−xLaYO3 (0≤x≤0.50) Ceramics. Journal of the American Ceramic Society, 93 (12), 4174-4181. [Article]

FORDER, S D, HANNANT, O M, BINGHAM, Paul and HAND, R J (2010). Concerning the use of standards for identifying coordination environments in glasses. Journal of Physics: Conference Series, 217, 012072. [Article]

FORDER, S D, HANNANT, O M, BINGHAM, Paul and HAND, R J (2010). Concerning the use of standards for identifying coordination environments in glasses. Journal of Physics : Conference Series, 217, 012072. [Article]

HASAN, Syed and SHAW, C.A. (2010). A method of analysis to predict fatigue life estimation of aluminium honeycomb/metallic foam core sandwich panels. In: AMPT 2010 : Advances in Materials and Processing Technologies, Paris, 24-27 October 2010. (Unpublished) [Conference or Workshop Item]

KARAGIANNI, E.T., MYRIOUNIS, Dimitrios, HASAN, Syed and MATIKAS, T.E. (2010). The thermomechanical processing effects of Al/SiCp composites under static loading testing. In: 1st Greek and Greek-Ukrainian Conference on Fracture Mechanics of Materials and Structures, Xanthi, Greece, 20-24 October 2010. (Unpublished) [Conference or Workshop Item]

LEWIS, O. D., GREENFIELD, D., AKID, R., DAHM, R. H. and WILCOX, G. D. (2010). Conversion coatings for zinc electrodeposits from modified molybdate solutions. Transactions of the Institute of Metal Finishing, 88 (2), 107-116. [Article]

LI, Ming, FETEIRA, Antonio, MIRSANEH, Mehdi, LANAGAN, Michael T. and SINCLAIR, Derek C. (2010). A link between p-type electrical conduction and microwave dielectric loss in highly ordered Ba(Co1/3Nb2/3)O3 ceramics. Journal of Materials Research, 25 (06), 1011-1014. [Article]

LI, Ming, FETEIRA, Antonio, MIRSANEH, Mehdi, LEE, Soonil, LANAGAN, Michael T., RANDALL, Clive A. and SINCLAIR, Derek C. (2010). Influence of nonstoichiometry on extrinsic electrical conduction and microwave dielectric loss of BaCo1/3Nb2/3O3 ceramics. Journal of the American Ceramic Society, 93 (12), 4087-4095. [Article]

LI, Shu-Xin, LI, Lei, YU, Shu-Rong, AKID, Robert and XIA, Hong-Bo (2010). Investigation of intergranular corrosion of 316L stainless steel diffusion bonded joint by electrochemical potentiokinetic reactivation. Corrosion Science. [Article]

LISHCHUK, S. V., MALOMUZH, N. P. and MAKHLAICHUK, P. V. (2010). Why thermodynamic properties of normal and heavy water are similar to those of argon-like liquids? Physics letters A, 374 (19-20), 2084-2088. [Article]

MAY, M., WANG, Heming and AKID, Robert (2010). Effects of the addition of inorganic nanoparticles on the adhesive strength of a hybrid sol–gel epoxy system. International Journal of Adhesion and Adhesives, 30 (6), p. 505. [Article]

MYRIOUNIS, Dimitrios (2010). Role of interfacial properties on the mechanical behaviour of Al/SiCp composites. In: IIMM 2010 : International Conference on Interfaces and Interphases in Multicomponent Materials, University of Sheffield, Sheffield, 1-3 September 2010. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios, HASAN, Syed and MATIKAS, T. E. (2010). Predicting interfacial strengthening behaviour of particulate-reinforced MMC : a micro-mechanistic approach. Composite Interfaces, 17 (4), 347-355. [Article]

MYRIOUNIS, Dimitrios, KORDATOS, E. Z., HASAN, Syed and MATIKAS, T. E. (2010). Crack-tip stress field and fatigue crack growth monitoring using infrared lock-in thermography in A359/SiCp composites. Strain, 47 (Supp 1), e619-e627. [Article]

VARGHESE, Jobin, JOSEPH, Tony, SEBASTIAN, Mailadil Thomas, REEVES-MCLAREN, Nik and FETEIRA, Antonio (2010). Crystal structure and microwave dielectric properties of LaLuO3 ceramics. Journal of the American Ceramic Society, 93 (10), 2960-2963. [Article]

WANG, H., AKID, R. and GOBARA, M. (2010). Scratch-resistant anticorrosion sol–gel coating for the protection of AZ31 magnesium alloy via a low temperature sol–gel route. Corrosion Science, 52 (8), 2565-2570. [Article]

2009

BINGHAM, Paul (2009). Design of new energy-friendly compositions. In: WALLENBERGER, Frederick T. and BINGHAM, Paul, (eds.) Fiberglass and glass technology : energy-friendly compositions and application. Springer, 267-354. [Book Section]

BINGHAM, Paul, CONNELLY, A.J., HAND, R.J., HYATT, N.C. and NORTHUP, P.A. (2009). Incorporation and speciation of sulphur in glasses for waste immobilisation. Glass technology, 50 (3), 135-138. [Article]

BINGHAM, Paul, HAND, R.J., HANNANT, O.M., FORDER, Sue and KILCOYNE, S.H. (2009). Effects of modifier additions on the thermal properties, chemical durability, oxidation state and structure of iron phosphate glasses. Journal of Non-Crystalline Solids, 355 (28-30), 1526-1538. [Article]

BRYANT, D. E., GREENFIELD, D., WALSHAW, R. D., EVANS, S. M., NIMMO, A. E., SMITH, C. L., WANG, L. M., PASEK, M. A. and KEE, T. P. (2009). Electrochemical studies of iron meteorites: phosphorus redox chemistry on the early Earth. International Journal of Astrobiology, 8 (1), 27-36. [Article]

FETEIRA, Antonio (2009). Negative Temperature Coefficient Resistance (NTCR) Ceramic Thermistors : an industrial perspective. Journal of the American Ceramic Society, 92 (5), 967-983. [Article]

FETEIRA, Antonio and SINCLAIR, Derek C. (2009). The influence of nanometric phase separation on the dielectric and magnetic properties of (1 − x)BaTiO3–xLaYbO3 (0 ≤ x ≤ 0.60) ceramics. Journal of Materials Chemistry, 19 (3), 356-359. [Article]

GITTENS, J. E., WANG, H., SMITH, T. J., AKID, R. and GREENFIELD, D. (2009). Biotic sol-gel coating for the inhibition of corrosion in seawater. ECS transactions, 24 (1), 211-229. [Article]

HANNANT, O. M., FORDER, Sue, BINGHAM, Paul and HAND, R. J. (2009). Structural studies of iron in vitrified toxic wastes. Hyperfine Interactions, 192 (1-3), 37-42. [Article]

HASAN, Syed and EASTERBRROK, L.E. (2009). Elastic-plastic thermal shock analysis : modelling of biaxial crack growth rates in thin 316 stainless steel plate. In: AMPT 2009 : Advances in Materials and Processing Technologies, Kuala Lumpur, Malaysia, 26-29 October 2009. (Unpublished) [Conference or Workshop Item]

KORDATOS, E. Z., MYRIOUNIS, Dimitrios, HASAN, Syed and MATIKAS, T. E. (2009). Monitoring the fracture behavior of SiCp/Al alloy composites using infrared lock-in thermography. In: WU, H. Felix, DIAZ, Aaron A., SHULL, Peter J. and VOGEL, Dietmar, (eds.) Nondestructive Characterization for Composite Materials, Aerospace Engineering, Civil Infrastructure, and Homeland Security 2009. Proceeding of SPIE (7294). SPIE. [Book Section]

LEWIS, O. D., CRITCHLOW, G. W. and WILCOX, G. D. (2009). The role of surface cleaning as a preliminary to satisfactory coating application. Corrosion management (89), 11-16. [Article]

LI, Ming, FETEIRA, Antonio and SINCLAIR, Derek C. (2009). Relaxor ferroelectric-like high effective permittivity in leaky dielectrics/oxide semiconductors induced by electrode effects: A case study of CuO ceramics. Journal of Applied Physics, 105 (11), p. 114109. [Article]

LI, Ming, SHEN, Zhijian, NYGREN, Mats, FETEIRA, Antonio, SINCLAIR, Derek C. and WEST, Anthony R. (2009). Origin(s) of the apparent high permittivity in CaCu[sub 3]Ti[sub 4]O[sub 12] ceramics: clarification on the contributions from internal barrier layer capacitor and sample-electrode contact effects. Journal of Applied Physics, 106 (10), p. 104106. [Article]

LISHCHUK, S. V. (2009). Saddle-splay modulus of a particle-laden fluid interface for hard disks. Europhysics Letters, 85 (5), p. 56001. [Article]

LISHCHUK, S. V. (2009). Scattering of light on surfactant-laden liquid-liquid crystal interface. Chemical Engineering Communications, 196 (7), 854-871. [Article]

LISHCHUK, S. V. (2009). Self-consistent field theory simulation of block copolymer films adsorbed on surfaces of azimuthally symmetric particles. Journal of Physics A: Mathematical and General, 42 (46), p. 465401. [Article]

LISHCHUK, S. V. and HALLIDAY, I. (2009). Effective surface viscosities of a particle-laden fluid interface. Physical review E. Statistical, nonlinear and soft matter physics, 80 (1), 016306. [Article]

MIRANDA, Laura, FETEIRA, Antonio, SINCLAIR, Derek C, BOULAHYA, Khalid, HERNANDO, Maria, RAMÍREZ, Julio, VARELA, Aurea, GONZÁLEZ-CALBET, Jose M. and PARRAS, Marina (2009). Composition−structure−property relationships of 6H- and 12R-Type Hexagonal Ba(Mn,Ti)O3−δPerovskites. Chemistry of Materials, 21 (8), 1731-1742. [Article]

MYRIOUNIS, Dimitrios, HASAN, Syed, BARKOULA, N.M., PAIPETIS, A. and MATIKAS, T.E. (2009). Effects of heat treatment on microstructure and the fracture toughness of SiCp/Al alloy metal matrix composites. Journal of advanced materials, 4 (3), 18-27. [Article]

RAWAL, Ritesh, MCQUEEN, Andrew J., GILLIE, Lisa J., HYATT, Neil C., MCCABE, Emma E, SAMARA, Kumaravinothan, ALFORD, Neil McN., FETEIRA, Antonio, REANEY, Ian M. and SINCLAIR, Derek C. (2009). Influence of octahedral tilting on the microwave dielectric properties of A[sub 3]LaNb[sub 3]O[sub 12] hexagonal perovskites (A=Ba, Sr). Applied Physics Letters, 94 (19), p. 192904. [Article]

SCHOFIELD, J.M., BINGHAM, Paul and HAND., R.J. (2009). The immobilisation of a chloride containing actinide waste surrogate in calcium aluminosilicate glasses. In: COZZI, Alex and OHJI, Tatsuki, (eds.) Environmental Issues and Waste Management Technologies in the Materials and Nuclear Industries XII. Ceramic Transactions (207). Wiley, 69-80. [Book Section]

WALLENBERGER, Frederick T. and BINGHAM, Paul (2009). Fiberglass and glass technology : energy-friendly compositions and applications. Springer. [Edited Book]

YANG, G., MOBUS, G., BINGHAM, Paul and HAND, R.J. (2009). Electron beam induced structure changes in borosilicate and borophosphate glasses: a comparison by energy loss spectroscopy. Physics and Chemistry of Glasses, 50 (6), 378-383. [Article]

2008

AKID, R. and WANG, H. (2008). Protective developments - Sol-gel systems show promise in antifouling and anticorrosive systems. European Coatings Journal, 5, 24-28. [Article]

AKID, R., WANG, H., SMITH, T. J., GREENFIELD, D. and EARTHMAN, J. C. (2008). Biological functionalization of a sol-gel coating for the mitigation of microbial-induced corrosion. Advanced functional materials, 18 (2), 203-211. [Article]

BINGHAM, Paul and HAND, R.J. (2008). Sulphate incorporation and glass formation in phosphate systems for nuclear and toxic waste immobilization. Materials Research Bulletin, 43 (7), 1679-1693. [Article]

BINGHAM, Paul, HAND, Russell J., STENNETT, Martin C., HYATT, Neil C. and HARRISON, Mike T. (2008). The use of surrogates in waste immobilization studies : a case study of plutonium. MRS Proceedings, 1107, 421-428. [Article]

BINGHAM, Paul, HYATT, Neil C, HAND, Russell J and WILDING, Christopher R (2008). Glass development for vitrification of Wet Intermediate Level Waste (WILW) from decommissionning of the Hinkley Point ‘A’ Site. MRS Proceedings, 1124. [Article]

BINGHAM, Paul and JACKSON, C.M. (2008). Roman blue-green bottle glass: chemical–optical analysis and high temperature viscosity modelling. Journal of Archaeological Science, 35 (2), 302-309. [Article]

BINGHAM, Paul, YANG, G., HAND, R.J. and MÖBUS, G. (2008). Boron environments and irradiation stability of iron borophosphate glasses analysed by EELS. Solid State Sciences, 10 (9), 1194-1199. [Article]

FETEIRA, Antonio and SINCLAIR, Derek C. (2008). Microwave dielectric properties of low firing temperature Bi2W2O9 ceramics. Journal of the American Ceramic Society, 91 (4), 1338-1341. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C., RAJAB, Khalid Z. and LANAGAN, Michael T. (2008). Crystal structure and microwave dielectric properties of Alkaline-Earth Hafnates, AHfO3(A=Ba, Sr, Ca). Journal of the American Ceramic Society, 91 (3), 893-901. [Article]

HANNANT, Oliver M., BINGHAM, Paul, HAND, Russell J. and FORDER, Sue D. (2008). A Mössbauer study of iron in vitrified wastes. MRS Proceedings, 1107, 215-222. [Article]

KRAWIEC, H., VIGNAL, V. and AKID, R. (2008). Numerical modelling of the electrochemical behaviour of 316 stainless steel based upon static and dynamic experimental microcapillary-based techniques: effect of electrolyte flow and capillary size. Surface and Interface Analysis, 40 (3-4), 315-319. [Article]

LARROUMET, D., GREENFIELD, D., AKID, R. and YARWOOD, J. (2008). Spectroscopic studies of the corrosion of model iron electrodes in carbonate and phosphate buffer solutions. Journal of Raman Spectroscopy, 39 (12), 1740-1748. [Article]

file
LISHCHUK, S. V., AKID, R. and WORDEN, K. (2008). Model-based prognosis for intergranular corrosion. Proc. 4th European Workshop on Structural Health Monitoring, Krakow, Poland, 340-348. [Article]

file
LISHCHUK, S. V., AKID, R. and WORDEN, K. (2008). A cellular automaton based model for predicting intergranular corrosion in aerospace alloys. Proc. EUROCORR–2008, Edinburgh, UK. [Article]

MIRANDA, Laura, FETEIRA, Antonio, SINCLAIR, Derek C., HERNÁNDEZ, Mar García, BOULAHYA, Khalid, HERNANDO, María, VARELA, Aurea, GONZÁLEZ-CALBET, Jose M. and PARRAS, Marina (2008). Study of the structural, magnetic, and electrical properties of the 5H Hexagonal-Type Perovskite BaMn0.2Co0.8O2.80. Chemistry of Materials, 20 (8), 2818-2828. [Article]

MYRIOUNIS, Dimitrios, HASAN, S. T. and MATIKAS, T. E. (2008). Influence of processing conditions on the micro-mechanical properties of particulate-reinforced aluminium matrix composites. Advanced composites letters, 17 (3), 75-85. [Article]

MYRIOUNIS, Dimitrios, HASAN, S. T. and MATIKAS, T. E. (2008). Microdeformationn behaviour of Al-SiC metal matrix composites. Composite Interfaces, 15 (5), 495-514. [Article]

MYRIOUNIS, Dimitrios, HASAN, Syed and MATIKAS, T. E. (2008). Heat treatment and interface effects on the mechanical behavior of SiC-particle reinforced aluminium matrix composites. Journal of ASTM International, 5 (7). [Article]

MYRIOUNIS, Dimitrios, HASAN, Syed and MATIKAS, T.E. (2008). Interfacial tailoring for the improvement of fatigue properties in SiC particulate reinforced aluminium matrix composites-NDE by heat wave detection. In: ECCM13 : 13th European Conference on Composite Materials, Royal Institute of Technology (KTH), Stockholm, Sweden, 2 - 5 June 2008. (Unpublished) [Conference or Workshop Item]

MÖBUS, G, TSAI, J, XU, XJ, BINGHAM, Paul and YANG, G (2008). Nanobead formation and nanopatterning in glasses. Microscopy and Microanalysis, 14 (S2), 434-435. [Article]

SCHOFIELD, James M., BINGHAM, Paul and HAND, Russell J. (2008). Waste loading of actinide chloride surrogates in an iron phosphate glass. MRS Proceedings, 1107, 253-260. [Article]

VOLOTINEN, T.T., PARKER, J.M. and BINGHAM, Paul (2008). Concentrations and site partitioning of Fe2+ and Fe3+ ions in a soda-lime-silica glass obtained by optical absorbance spectroscopy. Physics and Chemistry of Glasses, 49 (5), 258-270. [Article]

WANG, H. and AKID, R. (2008). Encapsulated cerium nitrate inhibitors to provide high-performance anti-corrosion sol-gel coatings on mild steel. Corrosion Science, 50 (4), 1142-1148. [Article]

ZHANG, Lwi, BEN, Liubin, THAKUR, Om Prakash, FETEIRA, Antonio, MOULD, Andrew G., SINCLAIR, Derek C. and WEST, Anthony R. (2008). Ferroelectric aging and recoverable electrostrain in BaTi0.98Ca0.02O2.98 ceramics. Journal of the American Ceramic Society, 91 (9), 3101-3104. [Article]

2007

AKID, R. (2007). Hybrid sol gel coatings are customized to fight corrosion. Materials performance, 46 (11), 14-15. [Article]

ATKINSON, J. D., CORRIGAN, M. R., HIGGINS, A. D. and ZHAO, Z. J. (2007). Interaction of EAC and DSA in C-Mn piping steels. In: 13th International Conference on Environmental Degradation of Materials in Nuclear Power Systems, Whistler, Canada, 19-23 August 2007. (Unpublished) [Conference or Workshop Item]

ATKINSON, J. D. and SAITHALA, J. R. (2007). Stress corrosion behaviour of super duplex stainless steel in dilute chloride solutions at 130C. In: Duplex 2007 International Conference and Expo, Grado, Italy, 18-20 June, 2007. (Unpublished) [Conference or Workshop Item]

ATKINSON, J.D. and SAITHALA, J. R. (2007). The effect of temperature and choride concentration on the pitting behaviour of Zeron100, 2205 and Ferralium Alloy255 duplex stainless steels. In: Duplex 2007 International Conference and Expo, Grado, Italy, 18-20 June, 2007. (Unpublished) [Conference or Workshop Item]

BINGHAM, Paul, CONNELLY, A.J., HAND, R.J., HYATT, N.C. and NORTHRUP, P.A. (2007). Solubility and speciation of sulphur in glasses for waste immobilization. In: Proceedings of the XXI International Congress on Glass: Strasbourg, France, 1 - 7 July 2007. Society of Glass Technology. [Book Section]

BINGHAM, Paul and HAND, R.J. (2007). Addition of P2O5 to SiO2-Al2O3-B2O3-MgO-CaO-Na2O glass : a study of its effects on glass properties, structure and melting behaviour. Glass technology, 48 (2), 78-88. [Article]

BINGHAM, Paul and HAND, R.J. (2007). Recycling of incinerator ashes : potential energy-saving raw materials for the manufactureof glasses and ceramics or simply low-grade aggregate materials? In: FREIMAN, S., (ed.) Proceedings of the 1st International Congress on Ceramics: A Global Roadmap. Wiley. [Book Section]

BINGHAM, Paul, PARKER, J.M., SEARLE, T.M. and SMITH, I. (2007). Local structure and medium range ordering of tetrahedrally coordinated Fe3+ ions in alkali–alkaline earth–silica glasses. Journal of Non-Crystalline Solids, 353 (24-25), 2479-2494. [Article]

FETEIRA, Antonio, GILLIE, Lisa J., ELSEBROCK, Ralf and SINCLAIR, Derek C. (2007). Crystal structure and dielectric properties of LaYbO3. Journal of the American Ceramic Society, 90 (5), 1475-1482. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C. and LANAGAN, Michael T. (2007). Structural and electrical characterization of CeAlO[sub 3] ceramics. Journal of Applied Physics, 101 (6), 064110. [Article]

LARROUMET, D., GREENFIELD, D., AKID, R. and YARWOOD, J. (2007). Raman spectroscopic studies of the corrosion of model iron electrodes in sodium chloride solution. Journal of Raman Spectroscopy, 38 (12), 1577-1585. [Article]

LI, Ming, FETEIRA, Antonio, SINCLAIR, Derek C. and WEST, Anthony R. (2007). Incipient ferroelectricity and microwave dielectric resonance properties of CaCu[sub 2.85]Mn[sub 0.15]Ti[sub 4]O[sub 12] ceramics. Applied Physics Letters, 91 (13), p. 132911. [Article]

LISHCHUK, S. V. (2007). Waves at surfactant-laden liquid-liquid crystal interface. Physical Review E (PRE), 76 (1), 011711. [Article]

LISHCHUK, S. V., LOKOTOSH, T. V., MAGAZU', S., MALOMUZH, N. P. and MIGLIARDO, F. (2007). Role of orientation disorder in the formation of fragility of glassy water and glycerol-like liquids. Physical Review E (PRE), 76 (6), 061504. [Article]

MIRANDA, Laura, BOULAHYA, Khalid, VARELA, Aurea, GONZÁLEZ-CALBET, José M., PARRAS, Marina, HERNANDO, María, FERNÁNDEZ-DÍAZ, M. Teresa, FETEIRA, Antonio and SINCLAIR, Derek C. (2007). Structure−property relationships of the 10H Hexagonal-Type Perovskite BaMn0.4Fe0.6O2.73. Chemistry of Materials, 19 (14), 3425-3432. [Article]

MYRIOUNIS, Dimitrios (2007). Microdeformation behaviour of Al-SiC metal matrix composites. In: 9th International Conference on Deformation & Fracture of Composites (DFC9), University of Sheffield, UK, 11-13 April 2007. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios (2007). Role of interfacial properties on the mechanical behaviour of Al-Sic metal-matrix composites. In: ICSAM 2007 - International Conference on Structural Analysis of Advanced Materials, Pathras, greece, 2-6 September 2007. (Unpublished) [Conference or Workshop Item]

MYRIOUNIS, Dimitrios, MATIKAS, T.E. and HASAN, Syed (2007). Microdeformation behaviour of Al-SiC metal matrix composite. In: COMP07 : omposites and applications for the new millennium : 6th International Symposium on Advanced Composites, Corfu Imperial Hotel, 16-18 May 2007. (Unpublished) [Conference or Workshop Item]

PASHA, U. M., ZHENG, H., THAKUR, O. P., FETEIRA, Antonio, WHITTLE, K. R., SINCLAIR, D. C. and REANEY, I. M. (2007). In situ Raman spectroscopy of A-site doped barium titanate. Applied Physics Letters, 91 (6), 062908. [Article]

RAY, B. C., HASAN, S. T. and CLEGG, D. W. (2007). Evaluation of defects in FRP composites by NDT techniques. Journal of Reinforced Plastics and Composites, 26 (12), 1187-1192. [Article]

SMITH, Alan (2007). The guiding light. Police professional: the professional journal of the UK police force (91), 24-26. [Article]

THAKUR, O.P., FETEIRA, Antonio, KUNDYS, B. and SINCLAIR, D.C. (2007). Influence of attrition milling on the electrical properties of undoped-BaTiO3. Journal of the European Ceramic Society, 27 (7), 2577-2589. [Article]

WANG, H. and AKID, R. (2007). A room temperature cured sol-gel anticorrosion pre-treatment for Al 2024-T3 alloys. Corrosion science, 49 (12), 4491-4503. [Article]

ZHANG, Lei, THAKUR, Om Prakash, FETEIRA, Antonio, KEITH, Gillian M., MOULD, Andrew G., SINCLAIR, Derek C. and WEST, Anthony R. (2007). Comment on the use of calcium as a dopant in X8R BaTiO[sub 3]-based ceramics. Applied Physics Letters, 90 (14), p. 142914. [Article]

2006

AKID, R. and WANG, H. (2006). Application of sol-gel technology for anticorrosion coatings and surface pretreatments. Galvanotechnik, 97 (9), 2098-2109. [Article]

AKID, R. and WANG, H. (2006). Sol-gel coatings: an alternative corrosion protection system. Corrosion Management (May/Ju), 9-12. [Article]

AKID, Robert, DMYTRAKH, I. M. and GONZALEZ-SANCHEZ, J. (2006). Fatigue damage accumulation: the role of corrosion on the early stages of crack development. Corrosion engineering science and technology, 41 (4), 328-335. [Article]

BINGHAM, Paul and HAND, R.J. (2006). Vitrification of toxic wastes : a brief review. Advances in Applied Ceramics: Structural, Functional and Bioceramics Journal - Advances in Psychiatric Treatment, 105 (1), 21-31. [Article]

BINGHAM, Paul, HAND, R.J. and FORDER, S.D. (2006). Doping of iron phosphate glasses with Al2O3, SiO2 or B2O3 for improved thermal stability. Materials Research Bulletin, 41 (9), 1622-1630. [Article]

BINGHAM, Paul, HAND, R.J., FORDER, S.D., LAVAYSIERRE, A, DELOFFRE, F, KILCOYNE, S.H. and YASIN, I. (2006). Structure and properties of iron borophosphate glasses. Physics and Chemistry of Glasses, 47 (4), 313-317. [Article]

BINGHAM, Paul, HAND, R.J., FORDER, S.D., LAVAYSIERRE, A., KILCOYNE, S.H. and YASIN, I. (2006). Preliminary studies of sulphate solubility and redox in 60P2O5–40Fe2O3 glasses. Materials Letters, 60 (6), 844-847. [Article]

BINGHAM, Paul, HAND, Russell J. and SCALES, Charlie R. (2006). Immobilisation of simulated plutonium-contaminated material in phosphate glass : an initial scoping study. MRS Proceedings, 932. [Article]

BRYANT, D. and GREENFIELD, D. (2006). The use of fluorescent probes for the detection of under-film corrosion. Progress in organic coatings. B, 57 (4), 416-420. [Article]

FERRARELLI, Matthew C., ADAMS, Timothy B., FETEIRA, Antonio, SINCLAIR, Derek C. and WEST, Anthony R. (2006). High intrinsic permittivity in Na[sub 1∕2] Bi[sub 1∕2] Cu[sub 3] Ti[sub 4] O[sub 12]. Applied Physics Letters, 89 (21), p. 212904. [Article]

FETEIRA, Antonio, ELSEBROCK, R., DIAS, A., MOREIRA, R.L., LANAGAN, M.T. and SINCLAIR, D.C. (2006). Synthesis and characterisation of La0.4Ba0.6Ti0.6RE0.4O3 (where RE=Y, Yb) ceramics. Journal of the European Ceramic Society, 26 (10-11), 1947-1951. [Article]

FETEIRA, Antonio, SINCLAIR, D. C. and LANAGAN, M. T. (2006). Microstructural and electrical characterisation of LaxBa1-xTi1-xYxO3 (0 <= x <= 0.50) ceramics. In: OHJI, T., SEKINO, T. and NIIHARA, K, (eds.) Science of Engineering Ceramics III : proceedings of the 3rd International Symposium. Key engineering materials (317-8). Trans Tech Pubn, 873-876. [Book Section]

FETEIRA, Antonio, SINCLAIR, Derek C. and LANAGAN, Michael T. (2006). Structure and microwave dielectric properties of Ca1?xYxTi1?xAlxO3 (CYTA) ceramics? [J. Mater. Res. 20, 2391 (2005)]. Journal of Materials Research, 21 (9), p. 2429. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C. and REANEY, Ian M. (2006). Synthesis and characterization of BaTi1-xGaxO3-delta (0x0.15) ceramics. Journal of the American Ceramic Society, 89 (7), 2105-2113. [Article]

HARRISON, Mike, SCALES, Charlie R., BINGHAM, Paul and HAND, Russell J. (2006). Survey of potential glass compositions for the immobilisation of the UK's separated plutonium stocks. MRS Proceedings, 985. [Article]

LEWIS, O. D., GREENFIELD, D., AKID, R., DAHM, R. H. and WILCOX, G. W. (2006). SVET investigation into use of simple molybdate passivation treatments on electrodeposited zinc coatings. Transactions of the Institute of Metal Finishing, 84 (4), 188-195. [Article]

LI, Ming, FETEIRA, Antonio, SINCLAIR, Derek C. and WEST, Anthony R. (2006). Influence of Mn doping on the semiconducting properties of CaCu3Ti4O12 ceramics. Applied Physics Letters, 88 (23), p. 232903. [Article]

LISHCHUK, S. V. (2006). Equation of state of the hard-disk fluid on a sphere from Percus–Yevick equation. Physica A Statistical Mechanics and its Applications, 369 (2), 266-274. [Article]

LISHCHUK, S. V. and CARE, C. M. (2006). A deformable elastic membrane embedded in a lattice Boltzmann fluid. arXiv:cond-mat/0607382v1. (Unpublished) [Article]

MYRIOUNIS, Dimitrios (2006). Role of segregation and precipitates of interfacial strengthening mechanism in Al-Sic MMC. In: Multiphase Materials, Knowledge Based Materials : Marie Cure Summer School, Sweden, 14-23 August 2006. (Unpublished) [Conference or Workshop Item]

PUNN, Rita, FETEIRA, Antonio, SINCLAIR, Derek C. and GREAVES, Colin (2006). Enhanced oxide ion conductivity in stabilized δ-Bi2O3. Journal of the American Chemical Society, 128 (48), 15386-15387. [Article]

RAWAL, Ritesh, FETEIRA, Antonio, FLORES, Alberto Arenas, HYATT, Neil C., WEST, Anthony R., SINCLAIR, Derek C., SARMA, Kumaravinothan and ALFORD, Neil McN. (2006). Dielectric properties of the "Twinned" 8H-Hexagonal Perovskite Ba8Nb4Ti3O24. Journal of the American Ceramic Society, 89 (1), 336-339. [Article]

RAWAL, Ritesh, FETEIRA, Antonio, HYATT, Neil C., SINCLAIR, Derek C., SARMA, Kumaravinothan and ALFORD, Neil McN. (2006). Microwave dielectric properties of hexagonal 12R-Ba3LaNb3O12 ceramics. Journal of the American Ceramic Society, 89 (1), 332-335. [Article]

SCHMITT, C., PLUVINAGE, G., HADJ-TAIEB, E. and AKID, R. (2006). Water pipeline failure due to water hammer effects. Fatigue and fracture of engineering materials and structures, 29 (12), 1075-1082. [Article]

2005

AKID, Robert, HOVSEPIAN, Papken and KOK, Y. N. (2005). Tribocorrosion testing of stainless steel (SS) and PVD coated SS using a modified scanning reference electrode technique. Wear, 259 (7-12), 1472-1481. [Article]

BINGHAM, Paul, FORDER, S. D., HAND, R. J. and LAVAYSIERRE, A. (2005). Mössbauer studies of phosphate glasses for the immobilisation of toxic and nuclear wastes. Hyperfine Interactions, 165 (1-4), 135-140. [Article]

BINGHAM, Paul and HAND, R (2005). Vitrified metal finishing wastes I. Composition, density and chemical durability. Journal of Hazardous Materials, 119 (1-3), 125-133. [Article]

BINGHAM, Paul, HAND, R.J., FORDER, S.D. and LAVAYSIERRE, A. (2005). Vitrified metal finishing wastes II. Thermal and structural characterisation. Journal of Hazardous Materials, 122 (1-2), 129-138. [Article]

BINGHAM, Paul and MARSHALL, M. (2005). Reformulation of container glasses for environmental benefit through lower melting temperatures. Glass technology, 46 (1), 11-19. [Article]

BLAZHNOV, I. V., MALOMUZH, N. P. and LISHCHUK, S. V. (2005). Dielectric permittivity of glycerol in the high viscosity region. Chemical Physics Letters, 418 (206), 230-234. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C. and LANAGAN, Michael T. (2005). Structure and microwave dielectric properties of Ca1− xY xTi1− xAl xO3 (CYTA) ceramics. Journal of Materials Research, 20 (09), 2391-2399. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C., REANEY, Ian M. and LANAGAN, Michael T. (2005). Structure-property relationships of BaTi1-2yGayNbyO3 (0<=y<=0.35) ceramics. Journal of the American Ceramic Society, 88 (11), 3055-3062. [Article]

LI, Ming, FETEIRA, Antonio and SINCLAIR, Derek C. (2005). Origin of the high permittivity in (La0.4Ba0.4Ca0.2)(Mn0.4Ti0.6)O-3 ceramics. Journal of Applied Physics, 98 (8), 084101-084101. [Article]

file
LISHCHUK, S. V., LOKOTOSH, T. V. and MALOMUZH, N. P. (2005). Properties of the H-bond network for two-dimensional lattice water model. Journal of Chemical Physics, 122 (24), p. 244504. [Article]

MOREIRA, R L, FETEIRA, Antonio and DIAS, A (2005). Raman and infrared spectroscopic investigations on the crystal structure and phonon modes of LaYbO3 ceramics. Journal of Physics - Condensed Matter, 17 (17), 2775-2781. [Article]

PETROYIANNIS, P. V., KERMANIDIS, A. T., AKID, R., RODOPOULOS, C. A. and PANTELAKIS, S. G. (2005). Analysis of the effects of exfoliation corrosion on the fatigue behaviour of the 2024-T351 aluminium alloy using the fatigue damage map. International Journal of Fatigue, 27 (7), 817-827. [Article]

REANEY, I M, IQBAL, Y, ZHENG, H, FETEIRA, Antonio, HUGHES, H, IDDLES, D, MUIR, D and PRICE, T (2005). Order-disorder behaviour in 0.9Ba([Zn0.60Co0.40](1/3)Nb-2/3)O-3-0.1Ba(Ga0.5Ta0.5)O-3 microwave dielectric resonators. Journal of the European Ceramic Society, 25 (7), 1183-1189. [Article]

2004

AKID, Robert and GARMA, M. (2004). Scanning vibrating reference electrode technique: a calibration study to evaluate the optimum operating parameters for maximum signal detection of point source activity. Electrochimica acta, 49 (17-18), 2871-2879. [Article]

BINGHAM, Paul (2004). The effects of 1 wt % P2O5 addition on the properties of container glass. Glass technology, 45 (6), 255-258. [Article]

file
BLAZHNOV, I. V., MALOMUZH, N. P. and LISHCHUK, S. V. (2004). Temperature dependence of density, thermal expansion coefficient and shear viscosity of supercooled glycerol as a reflection of its structure. The Journal of Chemical Physics, 121 (13), 6435-6441. [Article]

FETEIRA, Antonio, SINCLAIR, Derek C., REANEY, Ian M., SOMIYA, Yoshitaka and LANAGAN, Michael T. (2004). BaTiO3-Based ceramics for tunable microwave applications. Journal of the American Ceramic Society, 87 (6), 1082-1087. [Article]

HASAN, S. T., BEYNON, J. H. and FAULKNER, R. G. (2004). Role of segregation and precipitates on interfacial strengthening mechanisms in SiC reinforced aluminium alloy when subjected to thermomechanical processing. Journal of Materials Processing Technology, 153, 758-764. [Article]

XU, H., AKID, R. and BRUMPTON, G. (2004). Surface characterisation studies of CrVI and CrIII electroplated carbon steel samples. Transactions of the Institute of Metal Finishing, 82, 18-23. [Article]

XU, H., AKID, R., BRUMPTON, G., WANG, H. and RODENBURG, J. M. (2004). Electrochemical and AFM/SEM studies of Ni-Cr electroplated and sol-gel coated samples. In: MCVITIE, S. and MCCOMB, D., (eds.) Electron Microscopy and Analysis 2003. Institute of Physics Conference Series (179). CRC Press, 417-420. [Book Section]

2003

BINGHAM, Paul (2003). Container glass formulation : a fresh look at an old problem. Glass, 80, p. 336. [Article]

BINGHAM, Paul, PARKER, John M, SEARLE, Tim, WILLIAMS, John M and SMITH, Ian (2003). Novel structural behaviour of iron in alkali–alkaline-earth–silica glasses. Comptes Rendus Chimie, 5 (11), 787-796. [Article]

FETEIRA, Antonio, SARMA, Kumaravinothan, ALFORD, Neil McN., REANEY, Ian M. and SINCLAIR, Derek C. (2003). Microwave dielectric properties of Gallium-Doped Hexagonal Barium Titanate ceramics. Journal of the American Ceramic Society, 86 (3), 511-513. [Article]

RAY, B. C., HASAN, S. T. and CLEGG, D. W. (2003). Effect of thermal shock on modulus of thermally and cryogenically conditioned Kevlar/polyester composites. Journal of materials science letters, 22 (3), 203-204. [Article]

WANG, H., HUANG, Y. Z., RODENBURG, J. M. and SIMMONDS, M. C. (2003). Synthesis of nanosize powders and thin films of Yb-doped YAG by sol-gel methods. Chemistry of materials, 15 (18), 3474-3480. [Article]

2002

FETEIRA, Antonio, KEITH, G.M., RAMPLING, M.J., KIRK, C.A., REANEY, I.M., SARMA, K., MC. ALFORD, N. and SINCLAIR, D.C. (2002). Synthesis and characterisation of Ga-doped hexagonal BaTiO3. Crystal Engineering, 5 (3-4), 439-448. [Article]

LISHCHUK, S. V. (2002). Lekner summation of dipolar interaction in quasi-two-dimensional simulations. Molecular Physics, 100 (24), 3789-3793. [Article]

WANG, H., SIMMONDS, M. C. and RODENBURG, J. M. (2002). Manufacturing of YbAG coatings and crystallisation of the pure and Li2O doped Yb2O3-Al2O3 system by a modified sol-gel method. Materials chemistry and physics, 77 (3), 802-807. [Article]

2001

AKID, Robert and MILLS, D. J. (2001). A comparison between conventional macroscopic and novel microscopic scanning electrochemical methods to evaluate galvanic corrosion. Corrosion science, 43 (7), 1203-1216. [Article]

BINGHAM, Paul, PARKER, J.M., SEARLE, T., WILLIAMS, J.M. and SMITH, I. (2001). Novel structural behaviour of iron in alkali-alkaline earth-silica glasses. In: Proceedings of the XIX International Congress on Glass, Edinburgh, July 2001. Society of Glass Technology. [Book Section]

HU, H. and AKID, R. (2001). Cathodic-polarization effects on the long/short corrosion-fatigue crack growth rate of an offshore steel. Materials science, 37 (6), 902-909. [Article]

VERMA, B. B., ATKINSON, J. D. and KUMAR, M. (2001). Study of fatigue behaviour of 7475 aluminium alloy. Bulletin of Materials Science, 24 (2), p. 231. [Article]

2000

BREEN, C., AKID, R., HABESCH, S. and SAMMON, C. (2000). How clean is clean? Materials World, 8 (4), 15-17. [Article]

MURTAZA, G. and AKID, R. (2000). Empirical corrosion fatigue life prediction models of a high strength steel. Engineering Fracture Mechanics, 67 (5), 461-474. [Article]

1999

BINGHAM, Paul, PARKER, J.M., SEARLE, T., WILLIAMS, J.M. and FYLES, K. (1999). Redox and clustering of iron in silicate glasses. Journal of Non-Crystalline Solids, 253 (1-3), 203-209. [Article]

1998

BINGHAM, Paul, PARKER, J.M., SEARLE, T., WILLIAMS, J.M. and FYLES, K. (1998). Redox and clustering of iron in silicate glasses. In: Proceedings of the XVIII International Congress on Glass, San Francisco, July 1998. Society of Glass Technology. [Book Section]

1997

BRAMHALL, Mike, ROBINSON, I.M. and SMITH, Alan, eds. (1997). Engineering education, increasing student participation : post conference proceedings : [conference held at] Sheffield Hallam University, Sheffield, England, 12-14 September 1994. Sheffield, Sheffield Hallam University. [Edited Book]

1996

WANG, Y. Z., AKID, R., CLARKE, A. and ATKINSON, J. D. (1996). Further observations of early fatigue crack development. Fatigue and fracture of engineering materials and structures, 19 (5), 623-627. [Article]

WANG, Y. Z., ATKINSON, J., AKID, R. and PARKINS, R. N. (1996). Crack interaction, coalescence and mixed mode fracture mechanics. Fatigue & Fracture Of Engineering Materials And Structures, 19 (1), 51-63. [Article]

1994

SMITH, Alan, ed. (1994). Engineering education, increasing student participation: proceedings: Sheffield Hallam University, Sheffield, England, 12-14 September 1994. Sheffield, Sheffield Hallam University. [Edited Book]

1991

SMITH, Alan and STRATTON, R P (1991). Thermal treatment, grain boundary composition and intergranular attack resistance of alloy 690. In: Proceedings of the fifth international symposium on environmental degradation of materials in nuclear power system water reactors. La Grange Park, Illinois, American Nuclear Society, 855-861. [Book Section]

1990

SMITH, Alan and STRATTON, R P (1990). Relationship between composition, microstructure and corrosion behaviour of alloy 690 steam generator tubing for PWR systems. In: CUBICCIOTTI, D, (ed.) Proceedings of the fourth international symposium on environmental degradation of materials in nuclear power systems - water reactors. Houston, Texas, National association of corrosion engineers. [Book Section]